Poor Fullness

2019-11-26 0

Poor Fullness — Phenomena, Causes and Solutions  

1、Problem:Poor fullness

2、Phenomenon:After drying, the gloss of the paint film is not good, and it appears wizened and not full phenomenon.

3、Causes and solutions

Causes

Solutions

The sprayed   paint film is too thin.

Increase the oil   output of the spray gun, slow down the spraying speed, and increase the   spraying times.

The substrate or   primer is not smooth and absorbs paint.

Thoroughly sand   or seal the uneven substrate and primer.

The paint has   low viscosity and excessive dilution.

Strictly follow   the process requirements for dilution.