Causes | Solutions |
Incomplete drying of primer | Strengthen curing (increase baking temperature, extend baking time, increase UV curing energy) |
The paint film is too thick and the internal drying is not complete. | Adjust the coating method and control the thickness of the paint film. |
The primer is dissolved by the solvent of the topcoat | Choose the matching primer. |
The top coating’s baking temperature is too high | Control the baking temperature of the top coating. |
Excessive use of thinner leads to incomplete solvent volatilization. | Reasonably adjust the amount of thinner added. |